Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.3 - 58.6 MPa
7000 - 8500 psi
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength
BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat..