Material Notes:
CALIBREâ„¢ 1080 DVD resin has been developed to meet the high demands of the modern Optical Media Industry and is suitable for standard CD molding (audio or ROM) as well as for recordable optical storage discs (CD-R, CD-RW, DVD, MO and PD).Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 80 g/10 min

@Load 1.20 kg,
Temperature 300 °C
80 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 58
58
ASTM D785
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength, Ultimate 48.3 MPa
7000 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ASTM D638
Elongation at Break 60 %
60 %
50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
50 mm/min; ASTM D638
Flexural Strength 100 MPa
14500 psi
3-points, 2 mm/min; ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
3-points, 2 mm/min; ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
278 °F
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
256 °F
unannealed; ASTM D648
Optical Properties Metric English Comments
Refractive Index 1.583
1.583
ASTM D542
Transmission, Visible 91 %
91 %
ASTM D1003