Material Notes:
Cleanroom PVC-C sheet material is designed to be the most economical choice in FM 4910 materials. Compression Polymers Corp's Cleanroom PVC-C has been audited and tested in accordance with the FM 4910 protocol. It meets the test criteria with an FPI of 2 (limit of 6 max) and an SDI of 0.1 ( 0.4 max). PVC-C is FM listed.FEATURES AND BENEFITS Economics- The most economical sheet available for FM 4910 listed products. Weldability- Easy to fabricate with conventional welding equipment. It is also compatible with Corzan® 4910 CPVC. Strength- Superior physical characteristics to handle structural applications, inserts, machining, etc. Compatibility- Completely compatible with Corzan® 4910 CPVC systems and a broad range of semiconductor chemistry. Fire Safe- Listed in accordance to FM 4910 fire safe materials for clean room construction JI 3010757. Extruded Sheet- Extruded sheet offers the best surface quality and gauge consistency.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Ultimate 48.3 MPa
7000 psi
at 0.2"/min; ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
at 0.2"/min; ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
compression molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 124 µm/m-°C

@Temperature 20.0 °C
69.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability Test 0.060
0.060
SDI; UL 2360
0.10
0.10
SDI; FM 4910
1.6
1.6
FPI; UL 2360
2.0
2.0
FPI; FM 4910