Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 - 145 MPa
4000 - 21000 psi
Average value: 55.7 MPa Grade Count:33
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 100 - 145 MPa

@Temperature 130 - 180 °C
14500 - 21000 psi

@Temperature 266 - 356 °F
Average value: 84.7 MPa Grade Count:13
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Tensile Strength, Ultimate 100 - 145 MPa

@Time 1.80e+7 - 7.20e+7 sec
14500 - 21000 psi

@Time 5000 - 20000 hour
Average value: 84.7 MPa Grade Count:13
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Tensile Strength, Ultimate 135 - 145 MPa

@Temperature 130 - 180 °C
19600 - 21000 psi

@Temperature 266 - 356 °F
Average value: 107 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 135 - 145 MPa

@Time 1.80e+7 - 7.20e+7 sec
19600 - 21000 psi

@Time 5000 - 20000 hour
Average value: 107 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 55.0 - 145 MPa
7980 - 21000 psi
Average value: 117 MPa Grade Count:71
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Tensile Strength, Ultimate 60.0 - 145 MPa

@Temperature 60.0 - 150 °C
8700 - 21000 psi

@Temperature 140 - 302 °F
Average value: 108 MPa Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Tensile Strength, Ultimate 25.0 - 145 MPa

@Temperature -30.0 - 120 °C
3630 - 21000 psi

@Temperature -22.0 - 248 °F
Average value: 66.1 MPa Grade Count:1
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 25.0 - 145 MPa

@Strain 1.00 - 10.0 %
3630 - 21000 psi

@Strain 1.00 - 10.0 %
Average value: 66.1 MPa Grade Count:1
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 48.3 - 145 MPa
7000 - 21000 psi
Average value: 84.8 MPa Grade Count:33
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 30.0 - 145 MPa

@Temperature 60.0 - 150 °C
4350 - 21000 psi

@Temperature 140 - 302 °F
Average value: 78.6 MPa Grade Count:14
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Tensile Strength, Ultimate 114 - 145 MPa
16500 - 21000 psi
Average value: 131 MPa Grade Count:8
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Tensile Strength, Ultimate 93.1 - 145 MPa
13500 - 21000 psi
Average value: 122 MPa Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..
Tensile Strength, Ultimate 66.9 - 145 MPa
9700 - 21000 psi
Average value: 109 MPa Grade Count:17
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Tensile Strength, Ultimate 57.0 - 145 MPa
8270 - 21000 psi
Average value: 104 MPa Grade Count:24
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Tensile Strength, Ultimate 45.0 - 145 MPa

@Temperature -40.0 - 120 °C
6530 - 21000 psi

@Temperature -40.0 - 248 °F
Average value: 83.3 MPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..