Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.60 GPa | 1390 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,.. |
|||
Tensile Modulus | 9.60 GPa @Temperature 23.0 °C |
1390 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 |
Nilit FRIANYL A63 HS-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527-1/-2 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 Type 1A |
Solvay TECHNYL® R CR 218 V30 Nylon 6, 30% glass fiber, DRY TECHNYL® CR 218 V30 is a polyamide 6, reinforced with 30% glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color.Benefit.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific) Color Stable Glass filled PET |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East) Color Stable Glass filled PET |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9260DCS PET (Europe-Africa-Middle East) Color Stable Glass Filled PET (for Dark colors only) |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF0049SP PA 66 LNP* THERMOCOMP* RF0049SP is a compound based on Nylon 66 containing 20% Glass Fiber. Added features of this grade include: Flame Retardant, Heat Stabilized. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East) LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | DAM; ISO 527 2/1A |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527-2 |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527-1/-2 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ASTM D638 |
Plenco 4599 Phenolic, Granular, Injection Molded PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated .. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ASTM D638 |
Plenco 6582 Phenolic, Briquette, Injection Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | Transverse |
Goodfellow Polyaramid/Polyphenylene Sulfide Composite Sheet or Rod 25% Polyaramid fiber - PPS Matrix. Information provided by Goodfellow. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection mold.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 6635 A Nylon 66 Alloy, 35% Glass Fiber (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Modulus | 9.60 GPa | 1390 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |