Goodfellow Polyaramid/Polyphenylene Sulfide Composite Sheet or Rod

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Aramid Fiber Filled
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Polyaramid/Polyphenylene Sulfide Composite Sheet or Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% Polyaramid fiber - PPS Matrix. Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 83.0 MPa
12000 psi
Longitudinal
Elongation at Break 1.5 %
1.5 %
Tensile Modulus 9.60 GPa
1390 ksi
Transverse
Flexural Strength 124 MPa
18000 psi
Longitudinal
Flexural Modulus 7.60 GPa
1100 ksi
Longitudinal
Compressive Strength 76.0 MPa
11000 psi
Longitudinal
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Longitudinal