Plenco 4599 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4599 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated to provide improved cosmetic characteristics and mechanical strength properties. 04599 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.630 g/cc
0.0228 lb/in³
ASTM D1895
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Water Absorption 0.275 %
0.275 %
ASTM D570
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 108
108
ASTM D785
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 0.72 %
0.72 %
ASTM D638
Tensile Modulus 9.60 GPa
1390 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Compressive Strength 183 MPa
26500 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 3.56 GPa
516 ksi
Calculated
Izod Impact, Notched 0.162 J/cm
0.303 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.177 J/cm²
0.842 ft-lb/in²
ASTM D256
Impact 93
93
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.490 W/m-K

@Temperature 100 °C
3.40 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 202 °C
396 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 169 °C
336 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 29.2 %
29.2 %
ASTM D2863
Shrinkage 0.286 %
0.286 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.20e+11 ohm-cm
3.20e+11 ohm-cm
ASTM D247
Dielectric Constant 6.1
6.1
ASTM D150
Dielectric Strength 6.90 kV/mm
175 kV/in
Step by Step; ASTM D149
9.60 kV/mm
244 kV/in
Short Time; ASTM D149
Dissipation Factor 0.082
0.082
ASTM D150
Arc Resistance 159 sec
159 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638