Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/-2
Tensile Modulus 9.60 GPa
1390 ksi
ISO 527-1/-2
Flexural Strength 200 MPa
29000 psi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Flame Spread 54 mm/min

@Thickness 1.00 mm
2.1 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 20 %
20 %
ISO 4589-1/-2
Descriptive Properties Value Comments
Emission of organic compounds 91.4 µgC/g
VDA 277
Fogging 99%
ISO 6452; F-value (refraction)
Odour class 3
VDA 270
Part Marking Code >PBT-GF30<
ISO 11469
Processing Injection Moulding
Other Extrusion
Profile Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT-GF30
UL recognition UL
Copyright © lookpolymers.com All Rights Reserved