Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 V40 BLACK 21NHFE is characterized by a high flowability and offers an excellent combination between thermal and mechanical properties. This grade is ideal for use in the automotive industry for engine components, such as: inlet manifolds, air ducts - engine covers, and various housings and liquid containers. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
ISO 527 Type 1A
Elongation at Break 3.5 %
3.5 %
ISO 527 Type 1A
Tensile Modulus 9.60 GPa
1390 ksi
ISO 527 Type 1A
Flexural Strength 230 MPa
33400 psi
ISO 178
Flexural Modulus 7.60 GPa
1100 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.80 J/cm²
46.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: