Material Notes:
Type VI PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide range of aggressive chemical agentsUltra-low friction coefficientContinuous service temperature range from cryogenic -330°F to 500°FExtremely resistant to embrittlement, aging or weatheringPTFE has rapidly become the material choice where low friction, high durability, excellent thermal resistance and chemical inertness characteristics are required.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
Sintered moldings; ASTM D4894/D4895
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
DIN 53 466
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
Sintered molding, DIN 53 505
Tensile Strength, Ultimate 30.0 MPa

@Thickness 2.00 mm
4350 psi

@Thickness 0.0787 in
Sintered moldings; ASTM D4894/4895
Elongation at Break 450 %
450 %
Sintered Molding; ASTM D4894
Tensile Modulus 0.600 GPa
87.0 ksi
Sintered Molding, DIN 53457
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C

@Temperature 30.0 - 100 °C
66.7 µin/in-°F

@Temperature 86.0 - 212 °F
140 µm/m-°C

@Temperature 30.0 - 200 °C
77.8 µin/in-°F

@Temperature 86.0 - 392 °F
170 µm/m-°C

@Temperature 30.0 - 300 °C
94.4 µin/in-°F

@Temperature 86.0 - 572 °F
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
DIN 52 612
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service Temp
Minimum Service Temperature, Air -200 °C
-328 °F
Continuous Service Temp
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
IEC 60093
Copyright © lookpolymers.com All Rights Reserved