DSM Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
(DAM); ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527-1/-2
Elongation at Yield >= 50 %
>= 50 %
Nominal; ISO 527-1/-2
Tensile Modulus 0.600 GPa
87.0 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 12.5 J/cm²
59.5 ft-lb/in²
ISO 179/1eU
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
(DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
IEC 60093
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60243-1
Comparative Tracking Index 475 V
475 V
IEC 60112