Unitika EX-1030 PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Unitika
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika EX-1030 PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High-impact nylonInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 1.3 %

@Time 86400 sec
1.3 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 3.20 mm
0.012 in/in

@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 3.20 mm
0.016 in/in

@Thickness 0.126 in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ISO 2039
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO 527-1/-2
Elongation at Break >= 200 %
>= 200 %
ISO 527-1/-2
Tensile Modulus 0.600 GPa
87.0 ksi
ISO 527-1/-2
Flexural Strength 21.0 MPa
3050 psi
ISO 178
Flexural Modulus 0.600 GPa
87.0 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179-1
Charpy Impact, Notched NB
NB
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-2
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+12 ohm-cm
3.00e+12 ohm-cm
IEC 60093