Material Notes:
Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibilityLow fuel and freon permeabilityExcellent impact strength even at low temperatures Grilon BRZ 347 W is used typically for extruded and co-extruded tubes for fuel, freon and coolants.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 25.0 MPa
3630 psi
conditioned; ISO 2039-1
35.0 MPa
5080 psi
dry; ISO 2039-1
Tensile Stress 25.0 MPa

@Strain 50.0 %
3630 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
30.0 MPa

@Strain 50.0 %
4350 psi

@Strain 50.0 %
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
0.600 GPa
87.0 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 11.0 J/cm²
52.3 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
Melting Point 215 °C
419 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Air intake sytems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Processing Other Extrusion
Product Attributes Flexible
Special Characteristics High impact or impact modified
Copyright © lookpolymers.com All Rights Reserved