Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S USZ200 (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S USZ200 (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
(Dry)
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 30 %
30 %
Tensile Modulus 0.600 GPa
87.0 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 3.60 J/cm²

@Temperature -30.0 °C
17.1 ft-lb/in²

@Temperature -22.0 °F
13.0 J/cm²

@Temperature 23.0 °C
61.9 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved