Material Notes:
Fluoropolymer material specifications.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
ISO 12086
Water Absorption 0.020 %
0.020 %
DIN 53 495
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 65
60 - 65
DIN 53 505
Ball Indentation Hardness 25.0 - 30.0 MPa
3630 - 4350 psi
DIN 53 456
Tensile Strength 25.0 - 30.0 MPa
3630 - 4350 psi
DIN 53455
Elongation at Break 250 - 350 %
250 - 350 %
DIN 53455
Tensile Modulus 0.600 - 0.700 GPa
87.0 - 102 ksi
DIN 53457
Coefficient of Friction, Dynamic 0.25
0.25
on steel
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 - 100 °C
72.2 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Minimum Service Temperature, Air -200 °C
-328 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 50.0 - 80.0 kV/mm
1270 - 2030 kV/in
DIN 53481