Heat Stabilized
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
dry; ISO 1183
Moisture Absorption 3.70 %
3.70 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
cond; ISO 527-1/-2
100 MPa
14500 psi
dry; ISO 527-1/-2
30.0 MPa

@Temperature 200 °C
4350 psi

@Temperature 392 °F
ISO 527-1/-2
35.0 MPa

@Temperature 180 °C
5080 psi

@Temperature 356 °F
ISO 527-1/-2
40.0 MPa

@Temperature 160 °C
5800 psi

@Temperature 320 °F
ISO 527-1/-2
50.0 MPa

@Temperature 120 °C
7250 psi

@Temperature 248 °F
ISO 527-1/-2
Elongation at Break 40 %
40 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
cond; ISO 527-1/-2
>= 50 %

@Temperature 120 °C
>= 50 %

@Temperature 248 °F
ISO 527-1/-2
>= 50 %

@Temperature 160 °C
>= 50 %

@Temperature 320 °F
ISO 527-1/-2
>= 50 %

@Temperature 180 °C
>= 50 %

@Temperature 356 °F
ISO 527-1/-2
>= 50 %

@Temperature 200 °C
>= 50 %

@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus 1.00 GPa
145 ksi
cond; ISO 527-1/-2
3.30 GPa
479 ksi
dry; ISO 527-1/-2
0.500 GPa

@Temperature 200 °C
72.5 ksi

@Temperature 392 °F
ISO 527-1/-2
0.600 GPa

@Temperature 180 °C
87.0 ksi

@Temperature 356 °F
ISO 527-1/-2
0.650 GPa

@Temperature 160 °C
94.3 ksi

@Temperature 320 °F
ISO 527-1/-2
0.800 GPa

@Temperature 120 °C
116 ksi

@Temperature 248 °F
ISO 527-1/-2
Flexural Modulus 0.900 GPa
131 ksi
cond; ISO 178
3.30 GPa
479 ksi
dry; ISO 178
0.600 GPa

@Temperature 160 °C
87.0 ksi

@Temperature 320 °F
ISO 178
0.800 GPa

@Temperature 120 °C
116 ksi

@Temperature 248 °F
ISO 178
Izod Impact Resistance 0.400 J/cm²

@Temperature -40.0 °C
1.90 ft-lb/in²

@Temperature -40.0 °F
cond; ISO 180/1A
0.400 J/cm²

@Temperature -40.0 °C
1.90 ft-lb/in²

@Temperature -40.0 °F
dry; ISO 180/1A
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 180/1A
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
cond; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
cond; ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
dry; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
47.2 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 128 °C
262 °F
5000 hours Thermal Index; IEC 60216/ISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
dry; ISO 75-1/-2
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
dry; IEC 60695-11-10
V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
dry; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
cond; IEC 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
dry; IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
cond; IEC 60243-1
25.0 kV/mm
635 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
dry; IEC 60112