Material Notes:
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
Conditioned; ISO 868
83
83
ISO 868
Tensile Strength at Break 120 MPa
17400 psi
Conditioned; ISO R 527
195 MPa
28300 psi
ISO R 527
Elongation at Yield 2.0 %
2.0 %
ISO R 527
4.0 %
4.0 %
Conditioned; ISO R 527
Modulus of Elasticity 6.20 GPa
899 ksi
Conditioned; ISO 178
11.0 GPa
1600 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1A
23.0 kJ/m²
10.9 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/IeU
7.50 J/cm²
35.7 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/IeA
1.90 J/cm²
9.04 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
ASTM E831
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; CEI 60243-1
35.0 kV/mm
889 kV/in
CEI 60243-1
Comparative Tracking Index 550 V
550 V
CEI 60112/Solution A