Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.870 - 1.86 g/cc
0.0314 - 0.0672 lb/in³
Average value: 0.933 g/cc Grade Count:98
Viscosity 42.0 - 300000 cP

@Temperature 190 - 230 °C
42.0 - 300000 cP

@Temperature 374 - 446 °F
Average value: 40700 cP Grade Count:13
42.0 - 300000 cP

@Shear Rate 300 - 5000 1/s
42.0 - 300000 cP

@Shear Rate 300 - 5000 1/s
Average value: 40700 cP Grade Count:13
Environmental Stress Crack Resistance 1.00 - 1000 hour
1.00 - 1000 hour
Average value: 258 hour Grade Count:27
>= 1000 hour

@Temperature 50.0 - 50.0 °C
>= 1000 hour

@Temperature 122 - 122 °F
Average value: 668 hour Grade Count:2
4.00 - 4.00 hour

@Temperature 50.0 - 50.0 °C
4.00 - 4.00 hour

@Temperature 122 - 122 °F
Average value: 668 hour Grade Count:1
4.00 - 4.00 hour

@Thickness 3.80 - 3.80 mm
4.00 - 4.00 hour

@Thickness 0.150 - 0.150 in
Average value: 668 hour Grade Count:1
Thickness 25.4 - 38.1 microns
1.00 - 1.50 mil
Average value: 32.9 microns Grade Count:11
Melt Flow 0.800 - 150 g/10 min
0.800 - 150 g/10 min
Average value: 29.6 g/10 min Grade Count:95
Spiral Flow 32.0 - 67.8 cm
12.6 - 26.7 in
Average value: 47.6 cm Grade Count:10
Mechanical Properties Metric English Comments
Hardness, Shore D 44.0 - 70.0
44.0 - 70.0
Average value: 54.7 Grade Count:44
Tensile Strength, Ultimate 7.93 - 45.5 MPa
1150 - 6600 psi
Average value: 12.6 MPa Grade Count:38
Film Tensile Strength at Yield, MD 1.31 - 12.5 MPa
190 - 1810 psi
Average value: 9.65 MPa Grade Count:9
Film Tensile Strength at Yield, TD 10.3 - 13.0 MPa
1500 - 1890 psi
Average value: 12.0 MPa Grade Count:7
Tensile Strength, Yield 7.30 - 42.0 MPa
1060 - 6090 psi
Average value: 15.4 MPa Grade Count:68
Film Elongation at Break, MD 460 - 1000 %
460 - 1000 %
Average value: 677 % Grade Count:25
Film Elongation at Break, TD 540 - 1100 %
540 - 1100 %
Average value: 769 % Grade Count:23
Elongation at Break 25.0 - 1100 %
25.0 - 1100 %
Average value: 461 % Grade Count:60
Elongation at Yield 8.20 - 30.0 %
8.20 - 30.0 %
Average value: 13.1 % Grade Count:9
Modulus of Elasticity 0.140 - 1.57 GPa
20.3 - 227 ksi
Average value: 0.441 GPa Grade Count:25
Flexural Modulus 0.0165 - 0.758 GPa
2.40 - 110 ksi
Average value: 0.383 GPa Grade Count:55
Secant Modulus 0.230 - 0.689 GPa
33.4 - 100 ksi
Average value: 0.431 GPa Grade Count:10
Secant Modulus, MD 0.179 - 0.207 GPa
26.0 - 30.0 ksi
Average value: 0.201 GPa Grade Count:5
Secant Modulus, TD 0.221 - 0.238 GPa
32.0 - 34.5 ksi
Average value: 0.234 GPa Grade Count:5
Izod Impact, Notched 5.00 - 8.01 J/cm
9.37 - 15.0 ft-lb/in
Average value: 6.00 J/cm Grade Count:3
Izod Impact, Notched (ISO) 23.0 - 97.0 kJ/m²

@Temperature -50.0 - -50.0 °C
10.9 - 46.2 ft-lb/in²

@Temperature -58.0 - -58.0 °F
Average value: 44.5 kJ/m² Grade Count:8
Tensile Impact Strength 220.5 - 365.4 kJ/m²

@Temperature -40.0 - -40.0 °C
104.9 - 173.9 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 268 kJ/m² Grade Count:6
Dart Drop, Total Energy 2.44 J
1.80 ft-lb
Average value: 2.44 J Grade Count:4
Falling Dart Impact 27.1164 - 28.4722 J

@Temperature -40.0 - -40.0 °C
20.0000 - 21.0000 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 27.8 J Grade Count:2
Coefficient of Friction 0.120 - 0.500
0.120 - 0.500
Average value: 0.235 Grade Count:4
Coefficient of Friction, Static 0.200 - 0.580
0.200 - 0.580
Average value: 0.310 Grade Count:4
Elmendorf Tear Strength MD 260 - 600 g
260 - 600 g
Average value: 514 g Grade Count:12
Elmendorf Tear Strength TD 490 - 900 g
490 - 900 g
Average value: 729 g Grade Count:12
Elmendorf Tear Strength, MD 2.00 - 15.0 g/micron
50.8 - 381 g/mil
Average value: 7.72 g/micron Grade Count:11
Elmendorf Tear Strength, TD 7.30 - 27.6 g/micron
185 - 701 g/mil
Average value: 16.8 g/micron Grade Count:11
Dart Drop 3.00 - 19.7 g/micron
76.2 - 500 g/mil
Average value: 6.47 g/micron Grade Count:12
Dart Drop Test 290 - 1000 g
0.639 - 2.20 lb
Average value: 570 g Grade Count:12
Film Tensile Strength at Break, MD 21.0 - 56.5 MPa
3050 - 8200 psi
Average value: 38.7 MPa Grade Count:23
Film Tensile Strength at Break, TD 16.0 - 47.0 MPa
2320 - 6820 psi
Average value: 31.7 MPa Grade Count:23
Thermal Properties Metric English Comments
Melting Point 75.0 - 128 °C
167 - 262 °F
Average value: 113 °C Grade Count:36
Crystallization Temperature 106 - 111 °C
223 - 232 °F
Average value: 107 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 42.0 - 57.2 °C
108 - 135 °F
Average value: 48.9 °C Grade Count:11
Deflection Temperature at 1.8 MPa (264 psi) 35.0 - 35.6 °C
95.0 - 96.0 °F
Average value: 35.2 °C Grade Count:3
Vicat Softening Point 41.1 - 130 °C
106 - 266 °F
Average value: 96.1 °C Grade Count:62
Brittleness Temperature -76.1 - -27.0 °C
-105 - -16.6 °F
Average value: -68.0 °C Grade Count:32
Optical Properties Metric English Comments
Haze 1.50 - 55.0 %
1.50 - 55.0 %
Average value: 19.2 % Grade Count:17
Gloss 45.0 - 94.0 %
45.0 - 94.0 %
Average value: 67.2 % Grade Count:11
Processing Properties Metric English Comments
Nozzle Temperature 149 - 205 °C
300 - 401 °F
Average value: 198 °C Grade Count:8
Melt Temperature 95.0 - 302 °C
203 - 575 °F
Average value: 186 °C Grade Count:31
Mold Temperature 10.0 - 60.0 °C
50.0 - 140 °F
Average value: 36.6 °C Grade Count:7
Die Opening 0.0810 - 0.254 cm
0.0319 - 0.100 in
Average value: 0.169 cm Grade Count:6
Injection Pressure 2.76 - 100 MPa
400 - 14500 psi
Average value: 38.0 MPa Grade Count:5
Copyright © lookpolymers.com All Rights Reserved