Hannam Chemical Hanalac 780 ABS, High Flow

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Hannam Chemical
Trade Name Hanalac
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hannam Chemical Hanalac 780 ABS, High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys.
Physical Properties Metric English Comments
Melt Flow 5.5 g/10 min
5.5 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Notched 2.50 J/cm

@Thickness 3.17 mm
4.68 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Flammability, UL94 HB
HB