Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.0 - 7.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 - 7.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Terralene® WF 5525 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melt Flow | 6.1 - 7.5 g/10 min | 6.1 - 7.5 g/10 min | ASTM D1238-04 |
Ipiranga Petrochem GP 100 BK HDPE The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Melt Flow | 6.1 - 7.5 g/10 min | 6.1 - 7.5 g/10 min | ASTM D1238-04 |
Ipiranga Petrochem GP 100 OR HDPE The resin GP 100 OR is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min | 4.5 - 7.5 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPUP4G402 Polypropylene, 40% Talc Filled, High Flow Exceptional retention of mechanical properties and appearance upon long term heat aging.Applications: Appliance parts.Data provided by Washington Penn Plastic Co., Inc. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 5.5 - 7.5 g/10 min @Load 5.00 kg, Temperature 372 °C |
5.5 - 7.5 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Melt Flow | 2.5 - 7.5 g/10 min @Load 12.5 kg, Temperature 232 °C |
2.5 - 7.5 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Load 1.05 kg, Temperature 400 °C |
4.5 - 7.5 g/10 min @Load 2.31 lb, Temperature 752 °F |
ASTM D1238 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |