Eastman M30036-P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman M30036-P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
M30036-P is an extrusion coating performance polymer suggested for applications requiring performance similar to LLDPE. Compared to low density coating resins, M30036-P offers superior heat seal strength, as well as improved tensile strength, tear resistance, ESCR and abrasion resistance. Typical applications include laminates for nylon balloons, food pouches, cheese bags, potting soil bags, and hard-to-hold juice cans.Information supplied by the manufacturer.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D4883
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.50 MPa
1380 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 16.0 MPa
2320 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 58 %
58 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating