Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: FL 00623 is a good coextrusion partner in extrusion coating, blown and cast film. Excellent sealing material with a very low seal initiation temperature. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Applications:Adhesive Layer onto OPPBarrier Food PackagingCling LayerCoextrusion CoatingExtrusion CoatingExtrusion LaminationFlexible PackagingHigh Frequency SealingIndustrial PackagingInjection MoldingPVC ReplacementSurface Protection FilmWire and Cable CompoundsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ExxonMobil method
Vinyl Acetate Content 23 %
23 %
ExxonMobil method
Melt Flow 5.5 g/10 min
5.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85

@Time 15.0 sec
85

@Time 0.00417 hour
Molded Properties; ISO 868
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0303 GPa
4.40 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 172 °C
<= 342 °F
Peak Melting Point; ExxonMobil method
Crystallization Temperature <= 140 °C
<= 284 °F
Peak Temp; ASTM D3418
Vicat Softening Point 51.7 °C
125 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 230