Physical Properties Metric English Comments
Viscosity 6500 cP
6500 cP
NuSil MED-6607 Dispersion - Unrestricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Viscosity 6500 cP
6500 cP
NuSil MED10-6607 Dispersion - Restricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Viscosity 6500 - 10500 cP
6500 - 10500 cP
Huntsman Araldite GY 6008 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 177 to 188. Max color is 1.Comments/Applications: High purity, low viscosity, unmodified resin with very light color. General purpose resin. Solvent free and high s..
Viscosity 6500 - 8000 cP
6500 - 8000 cP
Huntsman Araldite PY 302-2 Bisphenol F Epoxy Resin
Weight per Epoxide (EEW, g/eq) 170 to 177. Max color is 3.Comments/Applications: Bisphenol A/F, non-crystallizing, low viscosity. Excellent mechanical properties. Used in coatings, adhesives, tan..
Viscosity 6500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
6500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2100203D2 Silver Ink
This product is part of a range of Heat Curable Inks. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has exce..
Viscosity 6500 cP
6500 cP
Mixed
Tra-Con Tra-Bond 2125NB Repair Epoxy Adhesive
TRA-BOND 2125NB is a high performance epoxy version of TRA-BOND 2125 formulated without micron-sized glass spheres. Information provided by Tra-Con Inc.
Viscosity 6500 cP

@Temperature 25.0 °C
6500 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive
TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an..
Viscosity 6500 cP

@Temperature 25.0 °C
6500 cP

@Temperature 77.0 °F
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Viscosity <= 6500 cP

@Temperature -40.0 °C
<= 6500 cP

@Temperature -40.0 °F
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684
ExxonMobil SpectraSyn™ 6 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) ..
Viscosity 6500 - 9500 cP

@Temperature 23.0 °C
6500 - 9500 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® H70E-2LC Thermally Conductive, Electrically Insulating Epoxy
Material Description: A two component, thermally conductive, electrically insulating epoxy designed for glob-top chip protection in TAB and COB die-attach technologies. It is used to prevent chips ..
Viscosity 6500 - 10500 cP

@Temperature 23.0 °C
6500 - 10500 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® P1011S Electrically Conductive Modified Polyimide
Product Description: EPO-TEK® P1011S is a single component, modified polyimide, high temperature grade, silver-filled electrically and thermally conductive adhesive designed for semiconductor die-a..
Viscosity 6500 - 10700 cP

@Temperature 23.0 °C
6500 - 10700 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste
Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec..
Viscosity 6500 - 8000 cP
6500 - 8000 cP
Abatron AboCast/AboCure 8109-9
Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°..
Viscosity 6500 - 7500 cP

@Temperature 35.0 °C
6500 - 7500 cP

@Temperature 95.0 °F
C.O.I.M. DIEXTER® G174 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Viscosity 6500 cP
6500 cP
3M Scotch-Weld™ MG6500-74 UV/VIS Medical Grade Light Cure Adhesive
3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing ..
Viscosity 6500 cP
6500 cP
Uncatalyzed, Deep Section Catalyst
ACC QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed..
Viscosity 6500 - 9500 cP
6500 - 9500 cP
Beijing Ranger Chem SM-826 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 6500 cP

@Temperature 25.0 °C
6500 cP

@Temperature 77.0 °F
at 100/35 (50-6/50-1) pbw
Abatron AboCast 50-6/AboCure 50-1 Epoxy
Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months.
Viscosity 6500 cP
6500 cP
uncatalyzed, Deep Section Catalyst
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting
QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C..
Viscosity 6500 cP
6500 cP
Loctite® 568 Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
Viscosity 6500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
6500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2090210P12 Silver Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Viscosity 6500 cP
6500 cP
uncatalyzed, Deep Section Catalyst
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting
QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section ..