Tra-Con Tra-Bond 2125NB Repair Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 2125NB Repair Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 2125NB is a high performance epoxy version of TRA-BOND 2125 formulated without micron-sized glass spheres. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Cured
Viscosity 6500 cP
6500 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
2 hrs @ 65°C
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Dark Gray
Mix Ratio, parts by weight 100/11
Resin/Hardener