Physical Properties Metric English Comments
Viscosity 7500 - 9500 cP
7500 - 9500 cP
Huntsman Araldite GY 6005 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 182 to 196. Max color is 1.Comments/Applications: Slightly modified GY 6010. Medium viscosity, general purpose, highly versatile resin for use in cold or heat-cured ..
Viscosity 5000 - 9500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
5000 - 9500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2000218D5 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 90/10. It is specifically designed to give good adhesion to ceramic substrates. Applications in medical diagnostics, environm..
Viscosity 7500 - 9500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
7500 - 9500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2050926P2 Lead-free Ag PZT Paste
This product is a Lead free termination for single layer PZT ceramics. After firing the film has good adhesion and solderability. Screen Printing Equipment: semi-automatic, manualScreen Types: stai..
Viscosity 6500 - 9500 cP
6500 - 9500 cP
Beijing Ranger Chem SM-826 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.