Material Notes:
Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months.
Physical Properties Metric English Comments
Viscosity 4000 - 6000 cP
4000 - 6000 cP
50-6
14000 - 20000 cP
14000 - 20000 cP
50-1
6500 cP

@Temperature 25.0 °C
6500 cP

@Temperature 77.0 °F
at 100/35 (50-6/50-1) pbw
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
Tensile Strength, Ultimate 46.95 MPa
6810 psi
Elongation at Break 2.0 %
2.0 %
Flexural Yield Strength 83.91 MPa
12170 psi
Flexural Modulus 2.25 GPa
326 ksi
Compressive Yield Strength 84.74 MPa
12290 psi
Compressive Modulus 1.65 GPa
239 ksi
Izod Impact, Notched 0.235 J/cm
0.440 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 92.0 °C
198 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 4.86e+15 ohm-cm
4.86e+15 ohm-cm
Surface Resistance 7.85e+15 ohm
7.85e+15 ohm
Dielectric Constant 2.95

@Frequency 1e+6 Hz
2.95

@Frequency 1e+6 Hz
3.2

@Frequency 1000 Hz
3.2

@Frequency 1000 Hz
3.24

@Frequency 60 Hz
3.24

@Frequency 60 Hz
Dissipation Factor 0.0097

@Frequency 60 Hz
0.0097

@Frequency 60 Hz
0.0097

@Frequency 1000 Hz
0.0097

@Frequency 1000 Hz
0.021

@Frequency 1e+6 Hz
0.021

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 160 min
160 min
500 g
Descriptive Properties Value Comments
Exotherm 153°C
Peak