Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6500 - 10500 cP | 6500 - 10500 cP | |
Huntsman Araldite GY 6008 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 177 to 188. Max color is 1.Comments/Applications: High purity, low viscosity, unmodified resin with very light color. General purpose resin. Solvent free and high s.. |
|||
Viscosity | 6500 - 8000 cP | 6500 - 8000 cP | |
Huntsman Araldite PY 302-2 Bisphenol F Epoxy Resin Weight per Epoxide (EEW, g/eq) 170 to 177. Max color is 3.Comments/Applications: Bisphenol A/F, non-crystallizing, low viscosity. Excellent mechanical properties. Used in coatings, adhesives, tan.. |
|||
Viscosity | 6500 - 8500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
6500 - 8500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2100203D2 Silver Ink This product is part of a range of Heat Curable Inks. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has exce.. |
|||
Viscosity | 6500 cP | 6500 cP | Mixed |
Tra-Con Tra-Bond 2125NB Repair Epoxy Adhesive TRA-BOND 2125NB is a high performance epoxy version of TRA-BOND 2125 formulated without micron-sized glass spheres. Information provided by Tra-Con Inc. |
|||
Viscosity | 6500 cP @Temperature 25.0 °C |
6500 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an.. |
|||
Viscosity | 6500 cP @Temperature 25.0 °C |
6500 cP @Temperature 77.0 °F |
|
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Viscosity | <= 6500 cP @Temperature -40.0 °C |
<= 6500 cP @Temperature -40.0 °F |
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684 |
ExxonMobil SpectraSyn™ 6 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Viscosity | 6500 - 10500 cP @Temperature 23.0 °C |
6500 - 10500 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® P1011S Electrically Conductive Modified Polyimide Product Description: EPO-TEK® P1011S is a single component, modified polyimide, high temperature grade, silver-filled electrically and thermally conductive adhesive designed for semiconductor die-a.. |
|||
Viscosity | 6500 - 10700 cP @Temperature 23.0 °C |
6500 - 10700 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |
|||
Viscosity | 6500 - 8000 cP | 6500 - 8000 cP | |
Abatron AboCast/AboCure 8109-9 Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°.. |
|||
Viscosity | 6500 - 7500 cP @Temperature 35.0 °C |
6500 - 7500 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G174 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 6500 cP | 6500 cP | |
3M Scotch-Weld™ MG6500-74 UV/VIS Medical Grade Light Cure Adhesive 3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing .. |
|||
Viscosity | 6500 cP | 6500 cP | Uncatalyzed, Deep Section Catalyst |
ACC QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed.. |
|||
Viscosity | 6500 - 9500 cP | 6500 - 9500 cP | |
Beijing Ranger Chem SM-826 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 6500 cP @Temperature 25.0 °C |
6500 cP @Temperature 77.0 °F |
at 100/35 (50-6/50-1) pbw |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |
|||
Viscosity | 6500 cP | 6500 cP | uncatalyzed, Deep Section Catalyst |
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C.. |
|||
Viscosity | 6500 cP | 6500 cP | |
Loctite® 568 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 6500 - 8500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
6500 - 8500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2090210P12 Silver Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 6500 cP | 6500 cP | uncatalyzed, Deep Section Catalyst |
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section .. |