Polymer Property : Viscosity = 10700 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 6500 - 10700 cP

@Temperature 23.0 °C
6500 - 10700 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste
Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec..
Viscosity 9300 - 10700 cP

@Temperature 35.0 °C
9300 - 10700 cP

@Temperature 95.0 °F
C.O.I.M. DIEXTER® G173 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..