Material Notes:
3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing component that allows for automated verification of adhesive dispensing. It has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable devices.Information provided by 3M
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Viscosity 6500 cP
6500 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 132 °C
270 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Optical Properties Metric English Comments
Refractive Index 1.467
1.467
Processing Properties Metric English Comments
Cure Time <= 0.0500 min
<= 0.000833 hour
Fixture Time, Glass side exposed to 10 mW/cm<sup>2</sup> @ 365 nm
Descriptive Properties Value Comments
Appearance Clear