Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7500 - 9500 cP | 7500 - 9500 cP | |
Huntsman Araldite GY 6005 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 182 to 196. Max color is 1.Comments/Applications: Slightly modified GY 6010. Medium viscosity, general purpose, highly versatile resin for use in cold or heat-cured .. |
|||
Viscosity | 5000 - 9500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
5000 - 9500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2000218D5 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 90/10. It is specifically designed to give good adhesion to ceramic substrates. Applications in medical diagnostics, environm.. |
|||
Viscosity | 7500 - 9500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
7500 - 9500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2050926P2 Lead-free Ag PZT Paste This product is a Lead free termination for single layer PZT ceramics. After firing the film has good adhesion and solderability. Screen Printing Equipment: semi-automatic, manualScreen Types: stai.. |
|||
Viscosity | 6500 - 9500 cP | 6500 - 9500 cP | |
Beijing Ranger Chem SM-826 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |