Material Notes:
QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. The 0.5% catalyst level can be increased or decreased to obtain desired cure speed. Cure speed can be accelerated by adding DBT catalyst in increments of 0.1%. QSil 60 can be catalyzed with 10% Deep Section Catalyst for application requiring a deeper cure. The material can also be vulcanized at elevated temperatures to increase cure speed.Key Features: Excellent thermal stability Self-leveling Variable cure speedPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
uncatalyzed, DBT Catalyst
1.47 g/cc
1.47 g/cc
uncatalyzed, Deep Section Catalyst
1.48 g/cc
1.48 g/cc
catalyzed
1.49 g/cc
1.49 g/cc
uncatalyzed
Viscosity 6500 cP
6500 cP
uncatalyzed, Deep Section Catalyst
55000 cP
55000 cP
Storage Temperature <= 4.00 °C
<= 39.2 °F
12 months
5.00 - 27.0 °C
41.0 - 80.6 °F
3 months
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
catalyzed, 24 hours
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
continuously and up to 316°C (600°F) intermittently
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Gel Time 45.0 min
45.0 min
Descriptive Properties Value Comments
Color Red