Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3000 cP | 3000 cP | Part B, RVT, #4, 2.5 rpm; TM R050-12 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Viscosity | 3000 cP @Temperature 190 °C |
3000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 2730 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good track, and very long open timeApplications: Component of hot me.. |
|||
Viscosity | 3000 cP @Temperature 190 °C |
3000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 4730 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Excellent low temperature flexibility, lower processing temperature, and superior adhesionApplications: Flooding and f.. |
|||
Viscosity | 3000 cP @Temperature 190 °C |
3000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 1230 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance, short open time, and excellent wetting propertiesApplications: Lamination of reinforced tapes and prot.. |
|||
Viscosity | 3000 - 3500 cP | 3000 - 3500 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 46-73/32 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa |
|||
Viscosity | 3000 - 7000 cP | 3000 - 7000 cP | |
Huntsman AroCy XU 71787.02 L Cyanate Ester Comments/Applications: Dicyclopentadiene based cyanate ester. Outstanding electrical properties. Low outgassing and equilibrium moisture absorption.Data provided by Ciba Specialty Chemicals.Ciba S.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | |
Huntsman HY 943 Aliphatic Amine Approx. H+ equivalent weight 38. Mix Ratio with GY 6010 is 20.Comments/Applications: Aliphatic amine adduct, light colored, very reactive. Coatings with excellent resistance to organic solvents a.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | 25% Toluene Solution; KM 06 |
Kraton® D1101 E (SBS) Liner Block Copolymer Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Viscosity | 3000 - 6000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
3000 - 6000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink UV curable Silver conductor ink specifically designed for printing on to polymeric substrates using flexographic printing. Ink can be printed at speeds up to 13m/min, with good line definition and .. |
|||
Viscosity | 3000 - 4000 cP @Time 7200 sec |
3000 - 4000 cP @Time 2.00 hour |
RP-0881 |
Solvay JAGUAR® C 14 S Surfactant Description: Substantive to hair and skin. Provides excellent wet combing and soft non-tacky feel to hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name : GUAR HYDROXYPROPYLTRIMONIUM CHLOR.. |
|||
Viscosity | 3000 - 15000 cP | 3000 - 15000 cP | |
Solvay POLYCARE® BOOST Surfactant Description: Water based emulsion of a high molecular weight linear polydimethylsiloxane containing a high delivery conditioning polymerC.T.F.A. /I.N.C.I. Name: WATER (AND) DIMETHICONE (AND) POLYQUA.. |
|||
Viscosity | 3000 cP @Temperature 25.0 °C |
3000 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 3000 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | >= 3000 cP | >= 3000 cP | 1% in Water After 60 min; RP-0945 |
Solvay AG-RHO™ DR-2000 Surfactant Chemical Name: COMPLEX CARBOHYDRATE POLYMER Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: AG-RHO® DR-2000 is a powdered form of HP guar for use as a drift reduc.. |
|||
Viscosity | 3000 - 10000 cP | 3000 - 10000 cP | LVT SSA #31 @ 3 rpm; RP-0596 |
Solvay RHODAPON® ALSA/K Surfactant Chemical Name: AMMONIUM LAURYL SULFATECAS: 68081-96-9 Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPON© ALSA/K is a primary surfactant providing excellen.. |
|||
Viscosity | 3000 cP | 3000 cP | |
Master Bond Mastersil 713 Low Viscosity One Component Silicone Master Sil 713 is a ready-to use, exceptionally low viscosity, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This .. |
|||
Viscosity | 3000 - 4800 cP @Temperature 150 °C |
3000 - 4800 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-15 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-15 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc.. |
|||
Viscosity | 3000 - 4800 cP @Temperature 150 °C |
3000 - 4800 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-15P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-15P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc.. |
|||
Viscosity | 3000 cP | 3000 cP | Haake cone and plate rheometer @ 5/sec (35mm/2° cone) |
Loctite® 3564 Fast flow epoxy, moderate CTE and Tg Fast Flow Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Viscosity | 3000 - 4000 cP @Temperature 23.0 °C |
3000 - 4000 cP @Temperature 73.4 °F |
|
Master Bond EP30DP Abrasion Resistant Cryogenic Epoxy Urethane System Master Bond Polymer System EP30DP is a versatile, two component, epoxy-urethane elastomeric compound, featuring superior strength, toughness, and abrasion resistance for high performance bonding, se.. |
|||
Viscosity | 3000 cP | 3000 cP | Mixed (cp #40, 5 rpm) |
Tra-Con Tra-Bond 516H03 Blush-Free Epoxy Adhesive TRA-BOND 516H03 is a modified version of F114 yielding a higher viscosity and lower coefficient of thermal expansion. Information provided by Tra-Con Inc. |
|||
Viscosity | 3000 cP | 3000 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7012 Release Modifier Syl-off® 7012 Release Modifier is a 100% active solids, pre-catalysed, release modifier. Offers particularly smooth release modification.Information provided by Dow Corning |
|||
Viscosity | 3000 - 6000 cP @Temperature 23.0 °C |
3000 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® M10-D Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Viscosity | 3000 cP | 3000 cP | |
Epoxyset Epoxiohm EO-24 Electrically Conductive Epoxy Adhesive EO-24 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management applica.. |
|||
Viscosity | 3000 cP | 3000 cP | Part B, RVT, #5, 20 rpm; TM R050-12 |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Viscosity | 3000 cP @Temperature 190 °C |
3000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 3330 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance temperature resistance and flexibilityApplications: Component of modified bitumen roofing systemsOth.. |
|||
Viscosity | 3000 cP | 3000 cP | Part B, RVT, #4, 2.5 rpm; TM R050-12 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |