Physical Properties Metric English Comments
Viscosity 3000 - 3500 cP
3000 - 3500 cP
15% solution in MEK
Lubrizol Advanced Materials Pearlstick® 46-73/32 Polyester based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa
Viscosity 1500 - 3500 cP

@Temperature 25.0 °C
1500 - 3500 cP

@Temperature 77.0 °F
Kinematic of 5.25% solution in Toluene
Sibur DST-30R-01 3rd Group Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE)
Kraton D 1184, 1186. As modifiers for bitumen for production of roofing materials, footwear compositions, adhesives, and coverings, as well as for modification of plastics. Addition of thermal ela..
Viscosity 1100 - 3500 cP
1100 - 3500 cP
Dynamic
Dow Corning Emulsifier 10 Emulsifier
Emulsifier designed to prepare water-in-oil and water-in-silicone emulsions for use in skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning
Viscosity 2000 - 3500 cP

@Temperature 23.0 °C
2000 - 3500 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H31LV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31LV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electron..
Viscosity 2900 - 3500 cP

@Temperature 60.0 °C
2900 - 3500 cP

@Temperature 140 °F
C.O.I.M. DIEXTER® G216 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Viscosity 200 - 3500 cP
200 - 3500 cP
Average value: 1830 cP Grade Count:12
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Viscosity 1300 - 3500 cP
1300 - 3500 cP
Huntsman Araldite GZ 488 V-32 US Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 3570 to 5500. Max color is 3.Comments/Applications: Very high molecular weight solid epoxy (8,000 - 10,000), 35% solids in PM acetate. Outstanding adhesion, excellen..
Viscosity 2000 - 3500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
2000 - 3500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2000802P2 Carbon Graphite Ink
This product is designed to be used for screen-printing working electrodes. This ink has been optimized to give superior electrochemical performance. It combines good line definition and good electr..