Tra-Con Tra-Bond 516H03 Blush-Free Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 516H03 Blush-Free Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 516H03 is a modified version of F114 yielding a higher viscosity and lower coefficient of thermal expansion. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Cured
Viscosity 3000 cP
3000 cP
Mixed (cp #40, 5 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
1 hr @ 65°C
80
80
24 hrs @ 25°C
Adhesive Bond Strength 26.5 MPa
3850 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
CTE, linear 42.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
23.3 µin/in-°F

@Temperature -40.0 - 32.0 °F
Alpha 1
Glass Transition Temp, Tg 52.0 °C
126 °F
Ultimate Tg; DSC
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Light Brown
Mixed