Physical Properties Metric English Comments
Viscosity 2000 - 4000 cP

@Temperature 25.0 °C
2000 - 4000 cP

@Temperature 77.0 °F
Uncured
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
Viscosity 3000 - 4000 cP

@Temperature 25.0 °C
3000 - 4000 cP

@Temperature 77.0 °F
Uncured
Resin Technology Group UV-422 Flexible, UV Curing Sealant
UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substr..
Viscosity 3000 - 4000 cP

@Temperature 25.0 °C
3000 - 4000 cP

@Temperature 77.0 °F
Uncured
Permabond UV640 UV-curable Adhesive
PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
Viscosity 50.0 - 4000 cP
50.0 - 4000 cP
Average value: 578 cP Grade Count:9
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Viscosity 3500 - 4000 cP
3500 - 4000 cP
as supplied
Industrial Nanotech Nansulateâ„¢ GP Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.NANSULATEâ„¢ liquid applied insulation is a prem..
Viscosity 3500 - 4000 cP
3500 - 4000 cP
as supplied
Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATEâ„¢ liquid applied insulation is a premium industrial grade rust proofing protective ..
Viscosity 3500 - 4000 cP
3500 - 4000 cP
as supplied
Industrial Nanotech Nansulateâ„¢ PT Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.NANSULATEâ„¢..
Viscosity 1500 - 4000 cP

@Temperature 40.0 °C
1500 - 4000 cP

@Temperature 104 °F
Taiwan PU Corporation PPG CPU-1060 Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Viscosity 3000 - 4000 cP
3000 - 4000 cP
30% solid in Anone
Taiwan Sheen Soon Sheenthane® A7020 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
Viscosity 3000 - 4000 cP

@Time 7200 sec
3000 - 4000 cP

@Time 2.00 hour
RP-0881
Solvay JAGUAR® C 14 S Surfactant
Description: Substantive to hair and skin. Provides excellent wet combing and soft non-tacky feel to hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name : GUAR HYDROXYPROPYLTRIMONIUM CHLOR..
Viscosity 2000 - 4000 cP
2000 - 4000 cP
ASTM D803
SK Chemicals SKYTHANE® U9081E Hardener
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Viscosity 2000 - 4000 cP

@Time 7200 sec
2000 - 4000 cP

@Time 2.00 hour
RP-0942
Solvay JAGUAR® C 17 Surfactant
Description: Highly substantive to hair and skin. Recommended for high conditioning shampoos and moisturizing body washes. Enhances deposition of actives such as silicone, anti-dandruff agents and m..
Viscosity 3000 - 4000 cP
3000 - 4000 cP
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable ..
Viscosity 1000 - 4000 cP
1000 - 4000 cP
mixed compound
Master Bond EP38CL Adhesive Features Toughness and Durability
Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura..
Viscosity 2000 - 4000 cP
2000 - 4000 cP
Part A
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound
Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no..
Viscosity 3000 - 4000 cP

@Temperature 23.0 °C
3000 - 4000 cP

@Temperature 73.4 °F
Master Bond EP21FL Flexibilized and Toughened Low Viscosity Epoxy
Master Bond Polymer System EP21FL is a lower viscosity, two component, flexibilized epoxy resin system for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at r..
Viscosity 3000 - 4000 cP

@Temperature 23.0 °C
3000 - 4000 cP

@Temperature 73.4 °F
Master Bond EP30DP Abrasion Resistant Cryogenic Epoxy Urethane System
Master Bond Polymer System EP30DP is a versatile, two component, epoxy-urethane elastomeric compound, featuring superior strength, toughness, and abrasion resistance for high performance bonding, se..
Viscosity 1000 - 4000 cP
1000 - 4000 cP
Part B
Master Bond EP30QF Quartz Filled, Two Component Epoxy System
Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at..
Viscosity 2800 - 4000 cP
2800 - 4000 cP
NOV QC 020
Lubrizol ESTANE® 5712F30 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Viscosity 2000 - 4000 cP

@Temperature 23.0 °C
2000 - 4000 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® EE149-6 Epoxy
Material Description: A single component, silver-filled, B-stageable epoxy designed for semiconductor flip chip packaging or hybrid micro-electronic substrate attach or lid-sealing.Information Provi..
Viscosity 3000 - 4000 cP

@Temperature 23.0 °C
3000 - 4000 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil..
Viscosity 2500 - 4000 cP

@Temperature 23.0 °C
2500 - 4000 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo..
Viscosity 2000 - 4000 cP

@Temperature 23.0 °C
2000 - 4000 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H61 Unfilled Epoxy Adhesive
Material Description: A single component, high Tg, electrically insulating epoxy adhesive for semiconductor, microelectronic, and opto-electronic packaging applications. It is a liquid version of E..
Viscosity 1000 - 4000 cP

@Temperature 25.0 °C
1000 - 4000 cP

@Temperature 77.0 °F
spindle n 3-10 RPM; MA143LFE
C.O.I.M. FILCO® 368 Film Former for Glass Fiber Sizes
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar..