Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3000 - 4800 cP @Temperature 150 °C |
3000 - 4800 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-15 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-15 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc.. |
|||
Viscosity | 3000 - 4800 cP @Temperature 150 °C |
3000 - 4800 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-15P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-15P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc.. |
|||
Viscosity | 1600 - 4800 cP | 1600 - 4800 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1052 Nitrile Elastomer Nipol 1052 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent general p.. |