Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV curable Silver conductor ink specifically designed for printing on to polymeric substrates using flexographic printing. Ink can be printed at speeds up to 13m/min, with good line definition and good conductivity. Flexographic Press Type: This product should has been designed to work on all types of flexo presses, with suitable UV driers. Substrate: Polyester, PolypropyleneInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 71.5 - 72.5 %

@Temperature 700 °C
71.5 - 72.5 %

@Temperature 1290 °F
Viscosity 3000 - 6000 cP

@Shear Rate 50.0 1/s,
Temperature 25.0 °C
3000 - 6000 cP

@Shear Rate 50.0 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 4.0 - 8.0 ohm
4.0 - 8.0 ohm
printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
11 - 22 ohm
11 - 22 ohm
printed onto 125µm PET film using 13cm<sup>3</sup>m<sup>-2</sup> anilox
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Cure Speed, m/min 13-16
Primarc P72 Mercury lamps 2 x 1.8Kw