Master Bond Mastersil 713 Low Viscosity One Component Silicone

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Mastersil 713 Low Viscosity One Component Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Sil 713 is a ready-to use, exceptionally low viscosity, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This compound is self leveling and can be readily applied to various surfaces.
Physical Properties Metric English Comments
Viscosity 3000 cP
3000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength, Yield 0.862 MPa
125 psi
Elongation at Yield 210 %
210 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -59.4 °C
-75.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Processing Properties Metric English Comments
Cure Time 720 - 1080 min

@Temperature 23.0 °C
12.0 - 18.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Translucent
Set-Up Time, minutes 6-8
At Room Temperature