Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
20000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | |
Huntsman Araldite EPN 1180 Epoxy Phenol Novolac Weight per Epoxide (EEW, g/eq) 175 to 182. Max color is 2.Comments/Applications: Epoxy functionality of 3.6. Much higher viscosity than EPN 1139 or EPN 1179. For higher heat and chemical resistan.. |
|||
Viscosity | 20000 - 80000 cP | 20000 - 80000 cP | |
Lord Adhesives 206 Long Working Time Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Viscosity | 20000 - 30000 cP | 20000 - 30000 cP | 30% solid in Anone/MEK |
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Viscosity | 20000 cP | 20000 cP | Before Curing |
Silikony Polskie Gumosil AD-1 A/B Silicone Rubber Flexible with high resistance to tension |
|||
Viscosity | 20000 - 30000 cP | 20000 - 30000 cP | Part A |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 286-5 Latex Emulsion TRA-BOND 286-5 latex emulsion is designed for temporary sealing of molds to prevent leaking during cure. This compound will thicken gradually due to water evaporation. Store containers with caps sec.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Trelleborg Emerson & Cuming Stycast® G-508-1 One-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Viscosity | 20000 cP | 20000 cP | Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Dow Corning BY 11-030 Silicone Surfactant A clear dispersion of a high molecular weight silicone surfactant in cyclopentasiloxane for use in skincare, suncare, shower gel, and color cosmetic applications. INCI Name: Cyclopentasiloxane (and).. |
|||
Viscosity | 20000 cP | 20000 cP | dynamic |
Dow Corning HS II BASE & 10:1 CLAY CATALYST High strength silicone mold making rubber, suited for the art foundry industry that typically uses sulfur-based clays. HS II Base with HS II 10:1 Clay Catalyst is recommended for use with polyesters.. |
|||
Viscosity | 20000 cP | 20000 cP | dynamic |
Dow Corning JCR 6101 UP One-part, translucent, thixotropic, medium modulus LED encapsulant which is a higher viscosity version of JCR 6101.Information provided by Dow Corning |
|||
Viscosity | 20000 - 80000 cP | 20000 - 80000 cP | dynamic |
Dow Corning Q2-7406 ADHESIVE Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning |
|||
Viscosity | 20000 - 90000 cP | 20000 - 90000 cP | dynamic |
Dow Corning Q2-7566 ADHESIVE Dow Corning® Q2-7566 Adhesive is a high viscosity, polydimethylsiloxane gum and resin dispersion, providing excellent high temperature properties with adhesion to 288C (550F).Information provided b.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Dymax 9001v3.5 Low Modulus Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9001v3.5 Low Modulus Clear MicroencapsulantLowest stress potting and encapsulation on ceramic, FR-4 or flexible PCBs.. |
|||
Viscosity | 20000 - 40000 cP @Temperature 21.0 °C |
20000 - 40000 cP @Temperature 69.8 °F |
|
Abatron AboCast/AboCure 8109-12 1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Armstrong A-702 Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Viscosity | 20000 cP | 20000 cP | |
ACC MM709 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 20000 cP | 20000 cP | Part B |
3M Scotchkote™ 323 Purple Patch Compound 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple.. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Viscosity | 20000 - 40000 cP | 20000 - 40000 cP | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 20000 cP @Temperature 105 °C |
20000 cP @Temperature 221 °F |
spindle #27, 18.7 grams, 5 rpm |
3M Dyneon™ FC 2210 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomers FC 2210 can be incorporated into other fluoroelastomers using standard water cooled internal mixers or two-roll mills
with standard fillers and ingredients utilized .. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
3M Scotch-Weld™ DP420 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Viscosity | 20000 cP | 20000 cP | |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Viscosity | 20000 - 40000 cP | 20000 - 40000 cP | |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 20000 cP | 20000 cP | Part A, RVT, #7, 20 rpm; TM R050-12 |
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje.. |
|||
Viscosity | 20000 cP | 20000 cP | Part B, RVT, #7, 20 rpm; TM R050-12 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | |
Beijing Ranger Chem SM-602RX75 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |