Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidly at elevated temperatures. It has a convenient one to one mix ratio by weight or volume. It has an unusual blend of properties including exceptionally high thermal conductivity, excellent electrical insulation properties, good physical strength and a high degree of flexibility. This system forms tough bonds that are resistant to shock, impact and thermal cycling as well as chemicals including water, oil and many solvents. EP37-3FLFAN has low viscosity with excellent flow characteristics making it ideal as a thermally conductive potting epoxy. It is cryogenically serviceable over the wide temperature range of 4K to 250°F. Part A is light gray and Part B is gray in color. Master Bond EP37-3FLFAN is widely used in the electronic, electrical, computer, metalworking, aerospace and chemical industries where electrical insulation and good heat transfer are required. The attractiveness of EP37-3FLFAN lies in the fact that this thermally conductive system retains a high level of flexibility while having the desirable physical characteristics inherent in epoxies. Product Advantages: Convenient mixing: easy-to-use, non-critical one to one mix ratio by weight or volume. Long working life; cures readily at room temperature and can be accelerated by heat. Good thermal conductivity with excellent electrical insulation properties. High bond strength to a wide variety of substrates; very good adhesive properties. Low viscosity with excellent flowability; ideal for potting and casting. Outstanding flexibility; resists rigorous thermal cycling, mechanical and thermal shocks. Good overall physical strength properties and chemical resistance. Cryogenically serviceable down to 4K.Information provided by MasterBond®
Physical Properties Metric English Comments
Viscosity 10000 - 20000 cP
10000 - 20000 cP
Part B
20000 - 30000 cP
20000 - 30000 cP
Part A
Mechanical Properties Metric English Comments
Hardness, Shore D 35 - 45
35 - 45
Tensile Strength at Break >= 27.6 MPa
>= 4000 psi
Shear Strength >= 6.21 MPa
>= 900 psi
Bond, Al to Al
Peel Strength >= 1.75 kN/m
>= 10.0 pli
T-peel, Al/Al
Thermal Properties Metric English Comments
CTE, linear 60.0 - 65.0 µm/m-°C
33.3 - 36.1 µin/in-°F
Thermal Conductivity 3.17 - 3.46 W/m-K
22.0 - 24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -168 °C
-270 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 5.1

@Frequency 60.0 Hz,
Temperature 25.0 °C
5.1

@Frequency 60.0 Hz,
Temperature 77.0 °F
Dielectric Strength 15.7 kV/mm

@Thickness 3.17 mm
400 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
2880 - 4320 min

@Temperature 23.9 °C
48.0 - 72.0 hour

@Temperature 75.0 °F
Pot Life 60 - 90 min
60 - 90 min
100 gram batch
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened container
Descriptive Properties Value Comments
Mixing Ratio (A to B) 1:1
by weight or volume