Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchkote™ 323 Purple Patch Compound

Category Other Engineering Material
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 323 Purple Patch Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple Patch Compound is the patch material color matched to 3M Scotchkote Fusion Bonded Epoxy.Information provided by 3M
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Viscosity 20000 cP
20000 cP
Part B
120000 cP
120000 cP
Part A
Mechanical Properties Metric English Comments
Abrasion 0.325
0.325
[g], CS-17 wheels, 1000g load, 5000 cycles wheels resurfaced every 500 cycles; ASTM D4060-95
Processing Properties Metric English Comments
Cure Time 26.0 min

@Temperature 50.0 °C
0.433 hour

@Temperature 122 °F
Dry to Touch Time; ASTM D1640 clause 7.5.2
39.0 min

@Temperature 50.0 °C
0.650 hour

@Temperature 122 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
105 min

@Temperature 24.0 °C
1.75 hour

@Temperature 75.2 °F
Dry to Touch Time; ASTM D1640 clause 7.5.2
159 min

@Temperature 24.0 °C
2.65 hour

@Temperature 75.2 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
420 min

@Temperature 5.00 °C
7.00 hour

@Temperature 41.0 °F
Dry to Touch Time; ASTM D1640 clause 7.5.2
480 min

@Temperature 5.00 °C
8.00 hour

@Temperature 41.0 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Purple