Material Notes:
1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:4 months/20°C (68°F), 1-2 months/40°C (105°F), 1-3 h/60°C (140°F); mix at RT; cures in: 3 h/140°C (285°F), 1 h/160°C (320°F), 30 min+1-3 h/180°C (355°F).Applications: Impregnating and laminating.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Viscosity 20000 - 40000 cP

@Temperature 21.0 °C
20000 - 40000 cP

@Temperature 69.8 °F
Vapor Pressure 0.00133 bar

@Temperature 180 °C
1.00 torr

@Temperature 356 °F
AboCast
<= 0.00533 bar

@Temperature 60.0 °C
<= 4.00 torr

@Temperature 140 °F
AboCure
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.16 MPa
8000 psi
Modulus of Elasticity 2.758 GPa
400.0 ksi
Flexural Yield Strength 89.63 MPa
13000 psi
Compressive Yield Strength 117.2 MPa
17000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 3.6 - 4.0

@Frequency 1e+6 Hz
3.6 - 4.0

@Frequency 1e+6 Hz
3.9 - 4.3

@Frequency 50 Hz
3.9 - 4.3

@Frequency 50 Hz
3.9 - 4.3

@Frequency 1000 Hz
3.9 - 4.3

@Frequency 1000 Hz
Dielectric Strength 13.78 - 15.75 kV/mm

@Thickness 3.17 mm
350.0 - 400.0 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0030 - 0.0070

@Frequency 50 Hz
0.0030 - 0.0070

@Frequency 50 Hz
0.0050 - 0.0090

@Frequency 1000 Hz
0.0050 - 0.0090

@Frequency 1000 Hz
0.020 - 0.040

@Frequency 1e+6 Hz
0.020 - 0.040

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Pot Life 60.0 - 180 min

@Temperature 100 °C
60.0 - 180 min

@Temperature 212 °F
43200 - 86400 min

@Temperature 40.0 °C
43200 - 86400 min

@Temperature 104 °F
>= 172800 min

@Temperature 20.0 °C
>= 172800 min

@Temperature 68.0 °F
>4 months