Material Notes:
High strength silicone mold making rubber, suited for the art foundry industry that typically uses sulfur-based clays. HS II Base with HS II 10:1 Clay Catalyst is recommended for use with polyesters, plaster, wax and cement and can be used with polyurethane.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc

@Temperature 25.0 °C
1.21 g/cc

@Temperature 77.0 °F
Viscosity 20000 cP
20000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 22
22
Tensile Strength, Ultimate 3.10 MPa
450 psi
Elongation at Break 325 %
325 %
Tear Strength 21.0 kN/m
120 pli
Descriptive Properties Value Comments
Mix Ratio (X:1) 10
Base to Catalyst ETN
Working Time (min) 45