Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thick.Availability:Asia PacificEuropeNorth America Additive:Flame RetardantLubricant Features:DuctileFlame RetardantGood Crack ResistanceGood Mold ReleaseGood ToughnessHalogen FreeHigh ElongationLow DensityLubricatedUses:AppliancesAutomotive ElectronicsBobbinsConnectorsElectrical HousingElectrical PartsElectrical/Electronic ApplicationsFastenersIndustrial ApplicationsLighting ApplicationsLiving HingesPrinted Circuit BoardsSwitchesAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Diameter 2.00 mm
0.012 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Diameter 2.00 mm
0.014 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ISO 527-2
Tensile Strength, Yield 52.0 MPa
7540 psi
ISO 527-2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527-2
Flexural Strength 45.0 MPa
6530 psi
ISO 178
Flexural Modulus 1.56 GPa
226 ksi
ISO 178