Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.010 - 0.017 cm/cm | 0.010 - 0.017 in/in | |
Custom Resins Vexel™ 3250 PBT
(discontinued **) General Purpose Unreinforced; High Flow. Property data for dry as molded samples.Data provided by the manufacturer |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.017 cm/cm | 0.016 - 0.017 in/in | ASTM D955 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latilub 66-20T PA66, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Time 86400 sec |
0.015 - 0.017 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Time 86400 sec |
0.015 - 0.017 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific) LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.017 cm/cm | 0.0080 - 0.017 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.017 cm/cm @Thickness 0.750 - 2.30 mm |
0.010 - 0.017 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.017 cm/cm @Thickness 0.750 - 2.30 mm |
0.010 - 0.017 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.017 cm/cm @Thickness 0.750 - 2.30 mm |
0.010 - 0.017 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.017 cm/cm @Thickness 3.18 mm |
0.015 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East) VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.017 cm/cm | 0.011 - 0.017 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LH-XE-NBK1 Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42L-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-NBK2 Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | ISO DIS 294-4 |
Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66 Description: Glass Sphere Filled, Toughened Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.017 cm/cm | 0.016 - 0.017 in/in | ASTM D955 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latishield 52/5-07A PP Homopolymer, Steel Fiber Reinforced EMI shielding product based on Polypropylene homopolymer (PPh). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ISO DIS 294-4 |
Wellman Wellamid® 42LH-NBK1 General Purpose Nylon 6 Description: General Purpose Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LH-WBK Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |