Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good WeatherabilityInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Melt Flow 9.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
9.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 142 MPa
20600 psi
5 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
5 mm/min; ASTM D638
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Flexural Modulus 13.7 GPa
1990 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.883 J/cm

@Thickness 6.35 mm
1.65 ft-lb/in

@Thickness 0.250 in
ASTM D256
1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.37 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
11.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C

@Thickness 6.40 mm
401 °F

@Thickness 0.252 in
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved