Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | |
Parker Chomerics CHO-SHIELD® 4914 Conductive Coating Conductive Solvent-Resistant Acrylic Coating. Formulated for high resistance to solvent attack, CHO-SHIELD® 4914 is an electrically conductive, one-component acrylic coating. Compared to zinc arc s.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ISO 1183 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ISO 1183 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc @Thickness 1.57 mm |
1.80 - 1.90 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe EP GC 22 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. High mechanical strength at elevated temperatures. Very good stability of .. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance. Information provided by Hippe. |
|||
Specific Gravity | 1.60 - 1.90 g/cc | 1.60 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe. |
|||
Specific Gravity | 1.60 - 1.90 g/cc | 1.60 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe SI MP 21 Mica Paper Reinforced Silicone Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 201 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature.Information provided by Hippe. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided .. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe EP GC 42 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at elevated temperatures. Very good stability of electrical properties when exposed to high relative .. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792-66 |
BCC Products Kwik Kast BC 8645 Urethane Casting BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792-66 |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |