Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer
Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co..
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite..
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer
Extruded onlyInformation provided by Chomerics
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi..
Specific Gravity 1.95 - 2.05 g/cc
1.95 - 2.05 g/cc
ISO 1183
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer
Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl..
Specific Gravity 2.03 - 2.05 g/cc
2.03 - 2.05 g/cc
ASTM D792
Adamas Adalon® 125 PTFE, 35% Carbon Filled
Information provided by Adamas, HPM
Specific Gravity 1.95 - 2.05 g/cc
1.95 - 2.05 g/cc
ASTM D792
Adamas Adalon® 401 PTFE, 10% Polyimide
Information provided by Adamas, HPM
Specific Gravity 1.95 - 2.05 g/cc
1.95 - 2.05 g/cc
ASTM D792
Adamas Adalon® 433 PTFE, 10% Ekonol®
Information provided by Adamas, HPM
Specific Gravity 1.90 - 2.05 g/cc
1.90 - 2.05 g/cc
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester
BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in..
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound
BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati..
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound
BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,..
Specific Gravity 1.95 - 2.05 g/cc
1.95 - 2.05 g/cc
Bulk Molding Compounds BMC 1050 Thermoset Polyester
BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e..
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester
BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel..