Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength, excellent overall electrical properties and flame resistance.Typical applications are circuit breakers, transformer bobbins, motor end bells and household appliances.
Physical Properties Metric English Comments
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Water Absorption 0.14 %
0.14 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 50
30 - 50
Tensile Strength, Ultimate 13.8 - 62.1 MPa
2000 - 9000 psi
Flexural Strength 75.8 - 145 MPa
11000 - 21000 psi
Izod Impact, Notched 2.67 - 8.01 J/cm
5.00 - 15.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0

@Thickness 6.35 mm
V-0

@Thickness 0.250 in
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Dielectric Strength >= 13.8 kV/mm
>= 350 kV/in
Short Time
Arc Resistance >= 170 sec
>= 170 sec
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F