Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ASTM D955
Multibase Nylex™ 2112 FR V0 Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Linear Mold Shrinkage 0.0050 - 0.013 cm/cm

@Thickness 3.17 mm
0.0050 - 0.013 in/in

@Thickness 0.125 in
Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66
Non-Hal red phosphorous based Flame Retardant CompoundAll properties after 48hrs conditioning at 23°C/50% RH
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
Across Flow; ISO 2577
Polykemi AB POLYelast TPE RCZ350D UV4 Thermoplastic Elastomer, UV-Resistant
Information provided by Polykemi AB
Linear Mold Shrinkage 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
Across Flow; ISO 2577
Polykemi AB POLYfill PPC T16020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH K20020 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0030 - 0.013 cm/cm
0.0030 - 0.013 in/in
ASTM D955
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2
Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment..
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D955
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0060 - 0.013 cm/cm
0.0060 - 0.013 in/in
FRISETTA Test Method
Nilit FRIANYL A63 HS-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0060 - 0.013 cm/cm
0.0060 - 0.013 in/in
FRISETTA Test Method
Nilit FRIANYL B63 HH-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0050 - 0.013 cm/cm
0.0050 - 0.013 in/in
FRISETTA Test Method
Nilit FRIANYL C73 TFGV1530 Nylon 6.6/6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced
Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0060 - 0.013 cm/cm
0.0060 - 0.013 in/in
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Linear Mold Shrinkage 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
ASTM D955
Kolon Kopa® KN161 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D955
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66
Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon.
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D1299
Loxim 811 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D1299
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ISO 2577
Polyram PlusTek PA350M4 Nylon 6.6 for Injection Molding, 20% Mineral Reinforced
20% Mineral Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm

@Thickness 3.20 mm
0.0090 - 0.013 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company ESD C 100 FR Polypropylene (PP); Flame Retardant - ESD Protection - Electrically Conductive
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm

@Thickness 3.17 mm
0.0090 - 0.013 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 132 Polypropylene (PP), Talc
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm

@Thickness 3.17 mm
0.0090 - 0.013 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 149 HB Polypropylene (PP), Mica - UL94 HB
RTP 149 HB is a mica reinforced polypropylene. It offers good strength, stiffness and improved heat distortion temperature vs. unreinforced polypropylene. Moldability, dimensional control and flat..
Linear Mold Shrinkage 0.0070 - 0.013 cm/cm

@Thickness 3.17 mm
0.0070 - 0.013 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 299 A X 92682 C Nylon 6 (PA), High Gravity Compound - Easy Molding
Linear Mold Shrinkage 0.0040 - 0.013 cm/cm
0.0040 - 0.013 in/in
ASTM D955
Beijing Ranger Chem PBT-MFC-G20 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
Across Flow; ISO 2577
Polykemi AB POLYfill PPHC K8030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm

@Thickness 3.17 mm
0.0090 - 0.013 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 132 Z Polypropylene (PP), Mineral - FDA Compliant Ingredients
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm

@Thickness 3.17 mm
0.0090 - 0.013 in/in

@Thickness 0.125 in
ASTM D955
RTP Company PermaStat® 4700  Polytrimethylene Terephthalate (PTT) Anti-Static  (discontinued
Anti-StaticComments:Permanently Anti-StaticESD ProtectionUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by..
Linear Mold Shrinkage 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
ASTM D955
Multibase Multi-Flam™ 1502 PP Black Polypropylene
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Copyright © lookpolymers.com All Rights Reserved